Abstract

In the spinel oxide cathode family, LiNi0.5Mn1.5O4 (LNMO) shows a high operating voltage (≈4.7 V vs Li/Li⁺) and excellent Li-ion mobility with stable 3D conducting channels. Ni/Mn cation disordered and ordered phases usually coexist in LNMO materials, and they have distinct structural and electrochemical properties, resulting in different battery performances for LNMO materials with different phase compositions. Identifying the correlation between phase compositions and electrochemical properties is of significance to the improvement of battery performance and understanding of degradation mechanisms. Herein, the disordered/ordered phase compositions in LNMO materials are tailored by post-annealing strategies and their impacts on electrochemical performance and degradation mechanisms from the surface to the bulk are systematically investigated. The ordered phase increases rapidly as Mn³⁺ is oxidized to Mn⁴⁺ through a post-annealing process. LNMO with an intermediate fraction of disordered and ordered phases gives rise to improved cycling stability. This article further reports that a high ordered phase fraction can preferentially protect Ni from dissolution during cycling. However, these results suggest that the transition metal dissolution and surface structural change of LNMO do not exhibit a direct correlation with cycling stability. These results indicate the capacity fading mainly correlates with the bulk structural distortion, leading to decreased Li-ion kinetics.

Tallennettuna:
Kysy apua / Ask for help

Sisältöä ei voida näyttää

Chat-sisältöä ei voida näyttää evästeasetusten vuoksi. Nähdäksesi sisällön sinun tulee sallia evästeasetuksista seuraavat: Chat-palveluiden evästeet.

Evästeasetukset